C |
Si |
Mn |
P |
S |
0.42~0.48 |
0.17~0.37 |
0.50~0.80 |
≤0.030 |
≤0.030 |
SM45钢的热加工工艺
项目 |
入炉温度/℃ |
加热温度/℃ |
开锻温度/℃ |
终锻温度/℃ |
冷却方式 |
钢锭 |
≤850 |
1150~1220 |
1100~1160 |
≥850 |
坑冷或堆冷 |
钢坯 |
|
1130~1200 |
1070~1150 |
≥850 |
坑冷或堆冷 |